PRINTING CONDITIONS
aMesh: 100-180 mesh
b superheat conditions: superheat 130-150 ℃ * 2 minutes
Printing process: printing → low temperature drying (natural dry) → over baking channel 130-150 ℃ * 2 minutes → completely dry after placing 4 hours to test the best results
MATTERS NEEDING ATTENTION
The total amount of color paste should not exceed 10% (ordinary colors are more likely to lead to the migration of the color of the paste, discoloration, it is recommended to use high temperature, migration-resistant color is better)
If you need to add auxiliaries before printing, you need to conduct a small test experiment in advance to determine the amount of addition can not exceed 1%.
After CG-180 add auxiliaries, it is forbidden to mix the slurry with auxiliaries into the original packaging barrel.
PRINTING SAMPLE TEST
Test Items | 180 | 检测方法 |
Covering power | ●●●●● | Internal standards: Level 5: very good / Level 4: very good / Level 3: good / Level 2: fair / Level 1: poor |
Softness | ●●●●● | Internal standards: Level 5: super soft / Level 4: softer / Level 3: soft / Level 2: average / Level 1: hard |
Color fastness to dry rubbing | Level 3.5 | GB-3920-2008,10 cycles of friction |
Color fastness to wet rubbing | Level 3.5 | GB-3920-2008,10 cycles of friction |
Machine wash fastness | pass | 8g Eagles phosphate-free laundry detergent, 60 ℃ water temperature * 95min / time, wash 5 times |
Cold resistance | - | Standard temperature -22℃ freezing for 24h |
Contact Us
Address:Building1,Zone1,Shenzhong Science and Technology Park,Sixth Industrial Zone ,Nanlang Town ,Zhongshan City,Guangdong
Company Tel:+86-0760-88209336
Company Fax:+86-0760-88665833
Scan Inquiry
Scan and download enterprise brochures on WeChat